Surface modification is one of the methods for improving the performance of medical implants inbiological environment. In this study, cerium, gallium and zinc substituted 80%SiO2-15%CaO-5%P2O5mesoporous bioactive glass (MBG) in combination with polycaprolactone (PCL) were coated over Ti6Al4 Vsubstrates by dip-coating method in order to obtain an inorganic—organic hybrid coating (MBG-PCL).Structural characterization was performed using XRD, nitrogen adsorption, SEM-EDXS, FTIR. The MBG-PCL coating uniformly covered the substrate with the thickness found to be more than 1 m. Glass andpolymer phases were detected in the coating along with the presence of biologically potent elementscerium, gallium and zinc. In addition, in vitro bioactivity was investigated by soaking the coated samplesin simulated body fluid (SBF) for up to 30 days at 37◦C. The apatite-like layer was monitored by FTIR, SEM-EDXS and ICP measurements and it formed in all the samples within 15 days except zinc samples. In thisway, an attempt was made to develop a new biomaterial with improved in vitro bioactive response dueto bioactive glass coating and good mechanical strength of Ti6Al4 V alloy along with inherent biologicalproperties of cerium, gallium and zinc.

Cerium, gallium and zinc containing mesoporous bioactive glasscoating deposited on titanium alloy

ANDREATTA, Francesco;FURLANI, Erika;MARIN, Elia;MASCHIO, Stefano;FEDRIZZI, Lorenzo
2016-01-01

Abstract

Surface modification is one of the methods for improving the performance of medical implants inbiological environment. In this study, cerium, gallium and zinc substituted 80%SiO2-15%CaO-5%P2O5mesoporous bioactive glass (MBG) in combination with polycaprolactone (PCL) were coated over Ti6Al4 Vsubstrates by dip-coating method in order to obtain an inorganic—organic hybrid coating (MBG-PCL).Structural characterization was performed using XRD, nitrogen adsorption, SEM-EDXS, FTIR. The MBG-PCL coating uniformly covered the substrate with the thickness found to be more than 1 m. Glass andpolymer phases were detected in the coating along with the presence of biologically potent elementscerium, gallium and zinc. In addition, in vitro bioactivity was investigated by soaking the coated samplesin simulated body fluid (SBF) for up to 30 days at 37◦C. The apatite-like layer was monitored by FTIR, SEM-EDXS and ICP measurements and it formed in all the samples within 15 days except zinc samples. In thisway, an attempt was made to develop a new biomaterial with improved in vitro bioactive response dueto bioactive glass coating and good mechanical strength of Ti6Al4 V alloy along with inherent biologicalproperties of cerium, gallium and zinc.
File in questo prodotto:
File Dimensione Formato  
Article APSUSC-Shruti.pdf

non disponibili

Tipologia: Versione Editoriale (PDF)
Licenza: Non pubblico
Dimensione 2.54 MB
Formato Adobe PDF
2.54 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11390/1081470
 Attenzione

Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo

Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 30
  • ???jsp.display-item.citation.isi??? 27
social impact