The present research compares properties and behaviour of co-precipitated 3Y-PSZ powders submitted, after co-precipitation, to different milling treatments. The characteristics of the different products were evaluated by measurement of particle size distribution, thermogravimetric analysis, X-ray diffraction, specific surface area and scanning electron microscopy analysis. It has been demonstrated that 1h of attrition milling enables the production of powders with micrometric particles: the dispersing liquid used on milling has little influence. Crystallization of the amorphous powder is achieved after 1h of high energetic milling, without any thermal treatment.
Production of 3Y-PSZ Powders by Co-precipitation and Milling
FURLANI, Erika;ANEGGI, Eleonora;MASCHIO, Stefano
2008-01-01
Abstract
The present research compares properties and behaviour of co-precipitated 3Y-PSZ powders submitted, after co-precipitation, to different milling treatments. The characteristics of the different products were evaluated by measurement of particle size distribution, thermogravimetric analysis, X-ray diffraction, specific surface area and scanning electron microscopy analysis. It has been demonstrated that 1h of attrition milling enables the production of powders with micrometric particles: the dispersing liquid used on milling has little influence. Crystallization of the amorphous powder is achieved after 1h of high energetic milling, without any thermal treatment.File | Dimensione | Formato | |
---|---|---|---|
Adv_scie_tecn_54_2008.pdf
non disponibili
Tipologia:
Versione Editoriale (PDF)
Licenza:
Non pubblico
Dimensione
1.59 MB
Formato
Adobe PDF
|
1.59 MB | Adobe PDF | Visualizza/Apri Richiedi una copia |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.